Figure 10.

a TEM image of gelatin-AgNPs synthesized at 90°C (Cgelatin: 0.4 wt%, <a onClick="popup('http://www.nanoscalereslett.com/content/6/1/22/mathml/M4','MathML',630,470);return false;" target="_blank" href="http://www.nanoscalereslett.com/content/6/1/22/mathml/M4">View MathML</a>: 2 mL); b XRD of gelatin-AgNPs power obtained from the sample in a; c TEM image of gelatin-AgNPs synthesized at 90°C (Cgelatin: 0.4 wt%, <a onClick="popup('http://www.nanoscalereslett.com/content/6/1/22/mathml/M4','MathML',630,470);return false;" target="_blank" href="http://www.nanoscalereslett.com/content/6/1/22/mathml/M4">View MathML</a>: 4 mL). AgNO3 was added in gelatin solution in two times. At first, 0.2 mL AgNO3 was added. The other AgNO3 was added into reaction mixture after 10 h.

Liu et al. Nanoscale Res Lett 2011 6:22   doi:10.1007/s11671-010-9756-1