Figure 3.

(a) XRD patterns of HA and YSZ/HA powder, with Ca/P ratio of 1,67 and YSZ content of 10%, heated at 950°C, 1 h in water vapor atmosphere, before indentation (b) and after indentation (c).

Vasconcelos and Barreto Nanoscale Res Lett 2011 6:20   doi:10.1007/s11671-010-9766-z