Resolution: standard / high Figure 3.
(a) XRD patterns of HA and YSZ/HA powder, with Ca/P ratio of 1,67 and YSZ content
of 10%, heated at 950°C, 1 h in water vapor atmosphere, before indentation (b) and
after indentation (c).
Vasconcelos and Barreto Nanoscale Res Lett 2011 6:20 doi:10.1007/s11671-010-9766-z |