Resolution: standard / high Figure 3.
Average size of gold nanoparticles in DI water measured by a Zetasizer (blue points
show the size of GNPs sonicated for 0, 30, and 45 min, and red points present the
size of GNPs using a mixed magnetic stirring and ultrasonication of total 30 min).
Chen and Wen Nanoscale Research Letters 2011 6:198 doi:10.1186/1556-276X-6-198 |