Figure 3.

Hardness versus strain rate of Ta films with d of 10 and 20 nm. The ml is determined from the slope of the lines. The inset shows the Young's modulus versus strain rate of Ta films with different values of d.

Cao et al. Nanoscale Research Letters 2011 6:186   doi:10.1186/1556-276X-6-186