Table 1 |
|||
|
FE parameters of Au film-coated SiNWs with different thicknesses |
|||
|
Samples |
Eon, (V/μm) |
EJ = 100μA/cm2 (V/μm) |
Φ (eV) |
|
|
|||
|
As-grown SiNWs |
5.01 |
5.93 |
4.15 |
|
Au20/SiNWs |
6.02 |
7.20 |
4.29 |
|
Au60/SiNWs |
6.03 |
7.81 |
4.51 |
|
Au80/SiNWs |
7.51 |
9.18 |
4.98 |
|
Au |
- |
- |
5.55 |
|
|
|||
|
Zhao et al. Nanoscale Research Letters 2011 6:176 doi:10.1186/1556-276X-6-176 |
|||