Figure 3.

Kelvin force microscopy surface potential maps after typical charging experiments. (a) up to ±20 V and (b) at ±25 V. Charging voltages are indicated near each stripe pattern.

Verveniotis et al. Nanoscale Research Letters 2011 6:144   doi:10.1186/1556-276X-6-144