Figure 2.

Pre-stretched thin membrane with an interface crack of length a. The membrane is subjected to a radial displacement of at its circumference outside the crack

Long et al. Nanoscale Research Letters 2010 5:1236-1239   doi:10.1007/s11671-010-9625-y