Figure 5.
The thin-walled index (TWI, defined as the ratio of inner diameter and wall thickness
of a CNT) of the CNTs produced at different temperatures: a 780°C, b 820°C, c 860°C
Cui et al. Nanoscale Research Letters 2010 5:941 doi:10.1007/s11671-010-9586-1 |