Table 1

Sample preparation and CVD conditions
Sample Grid material Ti(iOPr)4 coating method CVD temperature [°C]
1 Steel Dip 560
2 Steel Dip 640
3 Steel Dip 680
4 Steel Dip 760
5 Steel Dip 820
6 Steel Droplet 560
7 Steel Droplet 640
8 Steel Droplet 680
9 Steel Droplet 760
10 Steel Droplet 820
11 Ti Droplet 680
12 Ti Droplet 820
13 Si Spin 640

Colloid metal concentration used for support coating: 0.490 mg/ml

Engels et al. Nanoscale Research Letters 2010 5:904   doi:10.1186/1556-276X-5-904