Figure 7.

Frequency spectra of electric modulus M″ at 300°C in case of GDC0.2, EuDC0.2, and DyDC0.2 materials. Inset shows the Arrhenius plots of peak frequencies (fM″) in case of the EuDC0.2 and DyDC0.2 materials

Baral and Sankaranarayanan Nanoscale Research Letters 2010 5:637-643   doi:10.1007/s11671-010-9527-z