Figure 6.

Variation of real part of permittivity (ε′) with frequency at 400°C, in the case of GDC0.2, EuDC0.2, and DyDC0.2 materials

Baral and Sankaranarayanan Nanoscale Research Letters 2010 5:637-643   doi:10.1007/s11671-010-9527-z