Figure 5.

TEM images of CNTs grown at 5 Torr on the 2.7-nm (on left) and 4.7-nm (on right) thick Ni films

Kpetsu et al. Nanoscale Research Letters 2010 5:539-544   doi:10.1007/s11671-010-9544-y