Figure 3.

Initial Ni film thickness influence on final average Ni cluster size measured after H2 plasma pretreatment by AFM and SEM. Error bars indicate standard deviation of the grain size

Kpetsu et al. Nanoscale Research Letters 2010 5:539-544   doi:10.1007/s11671-010-9544-y