Figure 2.

AFM image of a 3.9-nm Ni film on a 100-nm TiN electrode after the pretreatment. The sample is the same as in image (d) of Fig. 1

Kpetsu et al. Nanoscale Research Letters 2010 5:539-544   doi:10.1007/s11671-010-9544-y