Figure 2.

Raman spectrum of CNTs before (a) and after (b) ALD of ZnO. Inset: Raman spectrum in the range of 150–650 cm−1 of ZnO-coated CNTs

Li et al. Nanoscale Research Letters 2010 5:1836-1840   doi:10.1007/s11671-010-9721-z