Figure 2.

Variations of a mean ledge thickness of nanowalls as a function of initial concentration of Zn(NO3)2·6H2O (mixed with a constant 0.1 M KCl) for a fixed deposition time of 20 min, and b film thickness of nanowalls deposited with 0.1 M Zn(NO3)2·6H2O (mixed with 0.1 M KCl) as a function of deposition time

Pradhan et al. Nanoscale Research Letters 2010 5:1727-1736   doi:10.1007/s11671-010-9702-2