Figure 6.

AFM images (a) and size distribution (b) of the nanoparticles formed by PAA-b-PEO-b-PAA (Ccopolymer = 1.0 g/L) and DTAB at DN =11

Peng et al. Nanoscale Research Letters 2009 5:89-95   doi:10.1007/s11671-009-9448-x