Figure 4.

Mass% increase of CNT paper after Pt deposition over 10 and 20 min, with the Fe foil no measurable increase was seen after 10 min

Petrik et al. Nanoscale Research Letters 2009 5:38-47   doi:10.1007/s11671-009-9440-5