Figure 3.

a SEM image of the freestanding ultrathin glassy carbon specimen mounted on the test device before loading. b The specimen after loading to fracture (scale bar is 50┬Ám)

Manoharan et al. Nanoscale Research Letters 2009 5:14-19   doi:10.1007/s11671-009-9435-2