Figure 8.
The specific magnetization of the MgFe2O4/PVP composite samples calcined in air for 2 h at different temperatures, as a function
of field, measured at 20 °C
Maensiri et al. Nanoscale Research Letters 2008 4:221 doi:10.1007/s11671-008-9229-y |