Figure 6.

XRD patterns of the MgFe2O4/PVP composite samples calcined in air for 2 h at different temperatures.a500 °C,b600 °C,c700 °C, andd800 °C

Maensiri et al. Nanoscale Research Letters 2008 4:221-228   doi:10.1007/s11671-008-9229-y