Figure 2.

TG-DTA curves of thermal decomposition of the as-spun MgFe2O4/PVP composite nanofibers at a heating rate of 5 °C/min in static air

Maensiri et al. Nanoscale Research Letters 2008 4:221-228   doi:10.1007/s11671-008-9229-y