Table 1 |
||
| Peak frequencies of Raman D and G mode of C–N nanotubes at three different growth temperatures | ||
| Growth temperature (°C) | Peak frequency (cm−1) | |
| D-mode | G-mode | |
| 850 | 1353.08 | 1578.36 |
| 900 | 1348.37 | 1573.28 |
| 950 | 1344.85 | 1569.32 |
Yadav et al. Nanoscale Research Letters 2008 4:197 doi:10.1186/1556-276X-4-197