SpringerOpen Newsletter

Receive periodic news and updates relating to SpringerOpen.

Open Access Nano Express

Ultra-Sensitivity Glucose Sensor Based on Field Emitters

Huibiao Liu1*, Xuemin Qian12, Shu Wang1, Yuliang Li1, Yinglin Song2 and Daoben Zhu1

Author Affiliations

1 CAS Key Laboratory of Organic Solid, Beijing National Laboratory for Molecular Sciences (BNLMS), Institute of Chemistry, Chinese Academy of Sciences, 100190, Beijing, People’s Republic of China

2 School of Physical Science and Technology, Suzhou University, 215006, Suzhou, Jiangsu, People’s Republic of China

For all author emails, please log on.

Nanoscale Research Letters 2009, 4:1141-1145  doi:10.1007/s11671-009-9372-0

The electronic version of this article is the complete one and can be found online at:


Received:4 May 2009
Accepted:2 June 2009
Published:14 June 2009

© 2009 to the authors

Abstract

A new glucose sensor based on field emitter of ZnO nanorod arrays (ZNA) was fabricated. This new type of ZNA field emitter-based sensor shows high sensitivity with experimental limit of detection of 1 nM glucose solution and a detection range from 1 nM to 50 μM in air at room temperature, which is lower than that of glucose sensors based on surface plasmon resonance spectroscopy, fluorescence signal transmission, and electrochemical signal transduction. The new glucose sensor provides a key technique for promising consuming application in biological system for detecting low levels of glucose on single cells or bacterial cultures.

Keywords:
ZnO nanorod arrays; Glucose sensor; Field emitter; High sensitivity

Introduction

The glucose sensors are becoming an increasingly active area of research due to their applications in biological, chemical analyze, and clinical detection [1]. Many glucose sensors based on surface plasmon resonance (SPR) spectroscopy [2,3], fluorescence signal transmission (FST) [4-8], and electrochemical signal transduction (EST) [9-11], have been reported. However, the sensitivity of these glucose sensors was mostly confined to the millimolar, which restricted their application in the case of lower glucose concentration, such as cellular signal transduction and protein biosynthesis in single cell or bacterial cultures. In order to further promote the sensitivity, intensive efforts have been made in the exploration of a glucose sensors based on nanostructured materials such as carbon nanotubes, semiconductor quantum dots, and nanowires [12-16].

Due to their unique properties of good biological compatibility and stability, nanomaterials of metal oxides could play an important role in adsorption of biomolecules. They are able to couple with different redox enzymes, which make them particular promising for their applications on biosensors and bioelectronics [17,18]. Being an important n-type semiconductor with a wide band gap (3.37 eV), ZnO possesses many versatile properties: high optical transparency, semiconducting, piezoelectric, nontoxicity, chemical stability, and electrochemical activity. Recently, one dimensional (1D) ZnO nanostructures for nanodevices such as field emitter [19], nanopiezotronics [20], gas and pH sensor [21], biosensor [22], transistor [23], and temperature laser [24], have received more and more attention due to their distinguished performance, high specific surface area, and facile preparation. 1D ZnO nanostructures have been used as electron mediators and adsorption matrices in amperometric biosensors [22]. Sun et al. [22,25,26] constructed a glucose amperometric biosensor using 1D ZnO nanostructures as supporting materials for glucose oxidase (GOx) loading, whose detection limit measured was 0.02 and 0.01 mM. Ren et al. [27] fabricated a ZnO nanorod-gated AlGa/GaN high electron mobility transistor for the detection of glucose, which showed a linear range from 0.01 to 3.45 mM. In this contribution, we present a new type of nanodevice, a glucose sensor based on field emitter of ZnO nanorod arrays (ZNA). The obvious changes of field emission properties of ZNA caused by surface energy band bending, which induced by surface adsorptions. This new ZNA field emitter-based sensor shows high sensitivity with an experimental limit of detection (LOD) of 1 nM glucose solution and a wide detection range from 1 nM to 50 μM in air at room temperature, which is lower than that of glucose sensor based on FST and EST.

Experimental Details

Materials and Apparatus

GOx(100 U mg−1) was purchased from Amersco Inc. (USA). All other reagents (analytical-grade) were purchased from Beijing Chemical Regent Company. The buffer solution was phosphate buffer (6 mM, pH 7.4). The water was purified using a Millipore filtration system.

The arrays of ZNA are characterized by field emission scanning electron microscopy (FESEM, Hitachi, S-4300). The field emission properties of ZNA are measured using a two-parallel-plate configuration in a homemade vacuum chamber at a base pressure of ~1.0×10−6 Pa at room temperature. The sample is attached to one of stainless-steel plates as cathode with the other plate as anode. The distance between the electrodes is 300 μm. A direct current voltage sweeping from 0 to 5,000 V was applied to the sample at a step of 50 V. The emission current is monitored using a Keithley 6485 picoammeter.

Synthesis of ZNA and Glucose Sensors

ZNA were directly grown on a Si (100) wafer with an area of 4 cm2 by a multi-step hydrothermal process [28]. The Si (100) wafer (4 cm2) is equably cut as 16 pieces of same area (0.5×0.5 cm2) samples. The samples for measurement of field emission were then prepared as follow: the films of Si (100) wafers deposited with ZNA were immersed in 2 mL Eppendorf cups with 10 μL of glucose oxidase (GOx) (10 U μL−1) and 1 mL of PBS buffer solution, respectively. Then the β-D-(+) glucose with different concentrations (from 1 nM to 50 μM) was added into the solution and incubated for 30 min at room temperature. After incubation, the samples were washed by pure water for three times. The samples were desiccated via vacuum for field emission measurement.

Results and Discussion

Figure 1a shows a typical SEM image of the as-grown ZNA prepared through hydrothermal process, which presents a rodlike morphology with a hexagonal cross-section. The nanorods are uniform on size with an average diameter of about 500 ± 10 nm. The cross-section of SEM image (Fig. 1b) demonstrates the nanorods are aligned along the perpendicular direction of the Si (100) wafer. The length of nanorods is about 6 μm.

thumbnailFigure 1. SEM images of ZNA:aTop view,bcross-section view

The field emission properties of the pure ZNA and ZNA film immersed with different concentrations glucose in PBS buffer solution are illustrated in Figs. 2a, b. As shown in Fig. 2a, the turn on field (Eto) of the film of pure ZNA is 5.83 V μm−1. The Eto values of ZNA immersed with 1, 10, 50, 100, and 250 nM glucose solution are 9.82, 9.96, 10.8, 10.97, 11.95 V μm−1, respectively. The control experiments show that the Eto values of ZNA immersing in PBS buffer solution, the glucose solution in PBS and the GOx solution in PBS and are 6.47, 6.5, and 6.83 V μm−1, respectively (Fig. 2b). These values are slightly bigger than that of pure ZNA. The Eto value of ZNA film immersed in 1 nM glucose solution increases obviously to 9.82 V μm−1, which is easily distinguished in comparison with that of pure ZNA (5.83 V μm−1). However, the measurement of field emission properties on the film of ZNA indicating no any signal was observed when the glucose concentration increased to 500 nM. This indicates that the experimental LOD is 1 nM, which is much lower compared with the glucose sensors based on GaN/AlGaN high electron mobility transistors [27].

thumbnailFigure 2. Field emission J–Ecurvesathe ZNA immersing in the glucose concentration from 1 to 500 nM in 6 mM PBS buffer solution and 10 U μL−1glucose oxidase with a pH value of 5.8.bThe control experiments, the ZNA immersing 6 mM PBS buffer solution, 1 mM glucose in 6 mM PBS buffer solution, 10 U μL−1glucose oxidase in 6 mM PBS buffer solution, respectively, with a pH value of 5.8

Figure 3a shows the R-M curve of the ZNA field emitters in different concentrations of 1 nM–50 μM glucose in PBS buffer and GOx solutions. It is clearly observed that the resistance of ZNA field emitter increases promptly with the increase of the glucose concentration. The resistance of the pure ZNA is about 650 Ω, which raises 9.3 times in the presence of 1 nM glucose (6,000 Ω) and about 12 times for 10 nM concentration of glucose (8,000 Ω). When the glucose concentration increases to 50 μM, the resistance is about 420 times that of the pure ZNA. However, the resistances of the ZNA in control experiments only increase slightly. Obviously, H2O2 that generated from the oxidation of glucose by the GOx catalyzed (Fig. 4) has strongly influence on the field emission property and conductivity of the ZNA. The ratio of Rglucose/RZnO for the ZNA field emitter-based glucose sensor presents a good dependence on the glucose concentrations (Fig. 3b). At this point, our ZNA field emitter-based glucose sensor surpasses previous glucose sensors based on many oxide semiconductors [22,25-27,29].

thumbnailFigure 3. aPlot of change resistance (R) as a function of concentrations (M) from 1 nM to 50 μM in 6 mM PBS buffer solution and 10 U μL−1glucose oxidase with a pH value of 5.8.bDependence relation between response sensitivity and glucose concentrations

thumbnailFigure 4. A schematic illustration of the ZNA field emitter-based glucose sensor operating principles

The properties of ZnO nanostructures are significantly influenced by surface adsorptions, which have been attracting great attention because the surface absorptions sometime disturb the fluorescence, field emission, and field effect transistors [30-32]. In general, the changes of properties caused by surface energy band bending, induced by surface adsorptions. As shown in Fig. 4, GOx specifically catalyzes the oxidation of β-D-(+)-glucose into gluconate and H2O2. H2O2 and ZnO to form ZnO(OH)x on the surface of ZnO nanorods [25], which depletes the electrons on the ZnO nanorods and yields oxygen ions (O, O2−, or O2) [33]. Leading to the electrons on the ZnO nanorods are trapped by the adsorbed oxygen molecules, and the surface depletion region of ZnO nanorods can be formed, making resistance increase. While the H2O2 is raised with the increase of glucose, more electrons are captured by the oxygen molecules at the nanorod surface. Thus, the surface depletion region is widened and the carrier density in the ZnO nanorod is decreased even more. At the same time, gluconolactone can be absorbed strongly on the surface of ZnO nanorods by hydrogen bonding with ZnO(OH)x, which induces the surface passivation to block the electrons emission of ZnO nanorods under electronic field. The surface passivation increases to completely deplete the electrons emission of ZnO nanorods with the increase of ZnO(OH)x on the surface of ZnO nanorods. The result indicates that field emission properties were not observed on the ZNA at the glucose concentration ≥500 nM.

Conclusions

In summary, we demonstrated a new glucose sensor based on the field emitter of ZNA. The results showed that a wide range of glucose concentrations from 1 nM to 50 μM is easily detected, which exhibits ultra-sensitivity for glucose detection. The experimental LOD of glucose concentration is 1 nM, which is lower than previous reported glucose sensor based on EST, FST, and SPR. The new glucose sensor shows the potential to detect low levels of glucose in biological system.

Acknowledgments

This work was supported by the National Nature Science Foundation of China (10874187 and 20873155) and the National Basic Research 973 Program of China.

References

  1. Rakow NA, Suslick KS:

    Nature. 2000, 406:710.

    COI number [1:CAS:528:DC%2BD3cXmt1CgsLw%3D]; Bibcode number [2000Natur.406..710R]

    PubMed Abstract | Publisher Full Text OpenURL

  2. Lee B, Perez-Luna VH:

    Anal. Chem.. 2005, 77:7204.

    COI number [1:CAS:528:DC%2BD2MXhtFSjtrnN]

    PubMed Abstract | Publisher Full Text OpenURL

  3. Aslan K, Lakowicz JR, Geddes CD:

    Anal. Chem.. 2005, 77:2007.

    COI number [1:CAS:528:DC%2BD2MXhtFeht7c%3D]

    PubMed Abstract | Publisher Full Text OpenURL

  4. Ge X-D, Tolosa L, Rao G:

    Anal. Chem.. 2004, 76:1403.

    COI number [1:CAS:528:DC%2BD2cXksFChtw%3D%3D]

    PubMed Abstract | Publisher Full Text OpenURL

  5. Meadows DL, Schultz JS:

    Talanta. 1988, 35:145.

    COI number [1:CAS:528:DyaL1cXitFygtL8%3D]

    PubMed Abstract | Publisher Full Text OpenURL

  6. Blagoi G, Rosenzweig N, Rosenzweig Z:

    Anal. Chem.. 2005, 77:393.

    COI number [1:CAS:528:DC%2BD2cXhtVCmsLnO]

    PubMed Abstract | Publisher Full Text OpenURL

  7. He F, Tang Y, Yu M, Wang S, Li Y, Zhu D:

    Adv. Funct. Mater.. 2006, 16:91.

    COI number [1:CAS:528:DC%2BD28XpvVWrsA%3D%3D]

    Publisher Full Text OpenURL

  8. He F, Feng F, Wang S, Li Y, Zhu D:

    J. Mater. Chem.. 2007, 17:3702.

    COI number [1:CAS:528:DC%2BD2sXps1Sns78%3D]

    Publisher Full Text OpenURL

  9. Chen W, Yao H, Tzang CH, Zhu J, Yang M, Lee S-T:

    Appl. Phys. Lett.. 2006, 88:213104.

    Bibcode number [2006ApPhL..88u3104C]

    Publisher Full Text OpenURL

  10. Chen T, Friedman KA, Lei I, Heller A:

    Anal. Chem.. 2000, 72:3757.

    COI number [1:CAS:528:DC%2BD3cXks1ehtr0%3D]

    PubMed Abstract | Publisher Full Text OpenURL

  11. Sapre AG, Bedekar A, Deshpande AV, Lali AM:

    Biotechnol. Lett.. 2000, 22:569.

    COI number [1:CAS:528:DC%2BD3cXjtlKmtLg%3D]

    Publisher Full Text OpenURL

  12. Wang J, Musameh M, Lin YH:

    J. Am. Chem. Soc.. 2003, 125:2408.

    COI number [1:CAS:528:DC%2BD3sXpvVartA%3D%3D]

    PubMed Abstract | Publisher Full Text OpenURL

  13. Duong HD, Il Rhee J:

    Talanta. 2007, 73:899.

    COI number [1:CAS:528:DC%2BD2sXht1SrurjO]

    PubMed Abstract | Publisher Full Text OpenURL

  14. Curreli M, Li C, Sun YH, Lei B, Gundersen MA, Thompson ME, Zhou CW:

    J. Am. Chem. Soc.. 2005, 127:6922.

    COI number [1:CAS:528:DC%2BD2MXjs1Sitr8%3D]

    PubMed Abstract | Publisher Full Text OpenURL

  15. Liu Y, Wang M, Zhao F, Xu Z, Dong S:

    Biosens. Bioelectron.. 2005, 21:984.

    COI number [1:CAS:528:DC%2BD2MXhtFKhsbjF]

    PubMed Abstract | Publisher Full Text OpenURL

  16. Yeh JI, Lazareck A, Ho Kim J, Xu J, Du S:

    Biosens. Bioelectron.. 2007, 23:568.

    COI number [1:CAS:528:DC%2BD2sXhtF2qt77K]

    PubMed Abstract | Publisher Full Text OpenURL

  17. Topoglidis E, Cass AEG, ORegan B, Durrant JR:

    J. Electroanal. Chem.. 2001, 517:20.

    COI number [1:CAS:528:DC%2BD3MXovFCmtLg%3D]

    Publisher Full Text OpenURL

  18. Yang YH, Yang HF, Yang MH, Liu YL, Shen GL, Yu RQ:

    Anal. Chim. Acta.. 2004, 525:213.

    COI number [1:CAS:528:DC%2BD2cXoslSms70%3D]

    Publisher Full Text OpenURL

  19. Xu CX, Sun XW:

    Appl. Phys. Lett.. 2003, 83:3806.

    COI number [1:CAS:528:DC%2BD3sXosF2ltrs%3D]; Bibcode number [2003ApPhL..83.3806X]

    Publisher Full Text OpenURL

  20. Wang ZL, Song JH:

    Science. 2006, 312:242.

    COI number [1:CAS:528:DC%2BD28XjtlKqu7g%3D]; Bibcode number [2006Sci...312..242W]

    PubMed Abstract | Publisher Full Text OpenURL

  21. Wang HT, Kang BS, Ren F, Tien LC, Sadik PW, Norton DP, Pearton SJ, Lin J:

    J. Appl. Phys. Lett.. 2005, 86:243503.

    Bibcode number [2005ApPhL..86x3503W]

    Publisher Full Text OpenURL

  22. Wang JX, Sun XW, Wei A, Lei Y, Cai XP, Li CM, Dong ZL:

    Appl. Phys. Lett.. 2006, 88:233106.

    Bibcode number [2006ApPhL..88w3106W]

    Publisher Full Text OpenURL

  23. Fan ZY, Lu JG:

    Appl. Phys. Lett.. 2005, 86:123510.

    Bibcode number [2005ApPhL..86l3510F]

    Publisher Full Text OpenURL

  24. Sun XW, Yu SF, Xu CX, Yuen C, Chen BJ, Li S:

    Jpn. J. Appl. Phys. 2.. 2003, 42:L1229.

    COI number [1:CAS:528:DC%2BD3sXosFSitbo%3D]

    Publisher Full Text OpenURL

  25. Wei A, Sun XW, Wang JX, Lei Y, Cai XP, Li CM, Dong ZL, Huang W:

    Appl. Phys. Lett.. 2006, 89:123902.

    Bibcode number [2006ApPhL..89l3902W]

    Publisher Full Text OpenURL

  26. Zang J, Li CM, Cui X, Wang JX, Sun XW, Dong H, Sun CQ:

    Electroanalysis. 2007, 19:1008.

    COI number [1:CAS:528:DC%2BD2sXls1ymtr4%3D]

    Publisher Full Text OpenURL

  27. Kang BS, Wang HT, Rena F, Pearton SJ, Morey TE, Dennis DM, Johnson JW, Rajagopal P, Roberts JC, Piner EL, Linthicum KJ:

    Appl. Phys. Lett.. 2007, 91:252103.

    Bibcode number [2007ApPhL..91y2103K]

    Publisher Full Text OpenURL

  28. Greene LE, Law M, Goldberger J, Kim F, Johnson JC, Zhang YF, Saykally RJ, Yang PD:

    Angew. Chem. Int. Ed.. 2003, 42:3031.

    COI number [1:CAS:528:DC%2BD3sXlslGksbw%3D]

    Publisher Full Text OpenURL

  29. Bao SJ, Li CM, Zang JF, Cui XQ, Qiao Y, Guo J:

    Adv. Funct. Mater.. 2008, 18:591.

    COI number [1:CAS:528:DC%2BD1cXjsVKmu7o%3D]

    Publisher Full Text OpenURL

  30. Bohle DS, Spina CJ:

    J. Am. Chem. Soc.. 2007, 129:12380.

    COI number [1:CAS:528:DC%2BD2sXhtVKmsbnE]

    PubMed Abstract | Publisher Full Text OpenURL

  31. Zhang Y, Kolmakov A, Chretien S, Metiu H, Moskovits M:

    Nano Lett.. 2004, 4:403.

    COI number [1:CAS:528:DC%2BD2cXosFKqsA%3D%3D]; Bibcode number [2004NanoL...4..403Z]

    Publisher Full Text OpenURL

  32. Song S, Hong WK, Kwon SS, Lee T:

    Appl. Phys. Lett.. 2008, 92:263109.

    Bibcode number [2008ApPhL..92z3109S]

    Publisher Full Text OpenURL

  33. Li QH, Liang YX, Wan Q, Wang TH:

    Appl. Phys. Lett.. 2004, 85:6389.

    COI number [1:CAS:528:DC%2BD2cXhtFSgu7rI]; Bibcode number [2004ApPhL..85.6389L]

    Publisher Full Text OpenURL