Figure 4.

Representative XPS spectrum of sample ZnS:Mn/ZnO(0.5) showing relative change in O/S atomic ratio with sputtering time

Jiang et al. Nanoscale Research Letters 2008 4:78-83   doi:10.1007/s11671-008-9205-6