Figure 6.
Decreased fibroblast density on silicone coated with Ti using ionic plasma deposition
after 1, 3, and 5 days. Data = mean ± STDEV, n = 3; *p < 0.01 (compared to silicone alone at the same time point); **p < 0.01 (compared to currently-used Ti at the same time point); and ***p < 0.01 (compared to previous time point on the same substrate)
Cohen et al. Nanoscale Research Letters 2007 2:385 doi:10.1007/s11671-007-9069-1 |